中国实用口腔科杂志

• 论著 • 上一篇    下一篇

钇稳定氧化锆全瓷冠与贵金属烤瓷冠抗折强度对照研究

罗玉玲1黄玮2a张强2b   

  1. 作者单位:1.江西省人民医院口腔一科,南昌330000;2.南昌大学附属口腔医院a优质门诊,b技工中心,南昌330000
  • 出版日期:2014-02-15 发布日期:2014-03-07

Flexural strength of Y-TZP all-ceramic crowns and precious metal ceramic restorations.

LUO Yu-lingHUANG WeiZHANG Qiang   

  1. *Department of Stomatology,the People’s Hospital of Jiangxi Province,Nanchang 330000,China
  • Online:2014-02-15 Published:2014-03-07

摘要:

目的 研究氧化锆全瓷冠与贵金属烤瓷冠抗折强度的差异。方法 在精密车床上模拟磨牙牙体预备制作金属基牙代型15个,分为3组。根据代型分别铸造金钯合金和金合金基底冠各5个,氧化锆全瓷冠5个。全部试件均黏固于代型上。采用电子万能测力仪测试试件抗折强度,即用直径5 mm的圆形加载头,以0.5 mm/min速度垂直加载于烤瓷冠牙合面中央至瓷层碎裂,记录瓷裂时强度值。采用单因素方差分析(One-way ANOVA)对各组数据进行分析。结果 金钯合金抗折强度为(3.932 ± 0.27)kN,金合金为(2.280 ± 0.20)kN,氧化锆为(2.08 ± 0.18)kN,金钯合金组抗折强度明显高于其他两组,差异有统计学意义(P < 0.05);金合金组和氧化锆组抗折强度值相近,差异无统计学意义(P > 0.05)。结论 研究条件下,金钯合金烤瓷冠抗折强度明显大于金合金烤瓷冠和氧化锆全瓷冠,而金合金烤瓷冠与氧化锆全瓷冠抗折强度则无明显差异。

关键词: 金合金, 金钯合金, 氧化锆, 抗折强度

Abstract:

Abstract:Objective To compare the flexural strength of Y-TZP all-ceramic crowns and two other different precious metals porcelain crowns. Methods Fifteen master tooth analogs were prepared resembling a molar crown preparation using the precision lathe and were divided into 3 groups.Five wax patterns were made from the mold and cast in a Au-Pd alloy,from which five Au-Pd metal-ceramic crowns were fabricated. Another 5 high-noble alloy metal-ceramic crowns and 5 ZrO2 all-ceramic were made from the same metal die.Each crown group were made in accordance with the specific manufacture’s instructions.All specimens were cemented on the analogs.Their fracture resistance was tested in a universal machine.A stainless steel rod with a 5-mm diameter stainless-steel ball was vertically placed on the occlusal surface of the crowns and at a speed of 0.5mm/min.Fracture was de?ned as occurrence of chipping.The loads at fracture were registered,and differences between the groups were calculated using One-way ANOVA. Results Au-Pd(3.932 ± 0.27)kN;Au(2.280 ± 0.20)kN;ZrO2(2.08 ± 0.18)kN. Significant differences in flexural strength between Au-Pd and other two groups were observed(P < 0.05),while there was no significant difference between the ZrO2 and high-noble group(P > 0.05).Conclusion Au-Pd group shows significantly greater flexural strength than high-noble and ZrO2 ceramic restorations(P < 0.05),while there's no significant difference between the ZrO2 and high-noble(P > 0.05).

Key words: high-noble alloy, Au-Pd, zirconia, flexural strength

中图分类号: